Alan Horowitz
2003-12-28 18:04:36 UTC
Permalink
how to sharpen the mini dike cutters and nipper cutters used in
electrical & electronic work?

They're too small to handle with jigs, and the blades don't even open
very widely. Yet, their utility is directly proportional to how
recently they've been sharpened/honed.
Don K
2003-12-28 18:21:17 UTC
Permalink
Post by Alan Horowitz
how to sharpen the mini dike cutters and nipper cutters used in
electrical & electronic work?
They're too small to handle with jigs, and the blades don't even open
very widely. Yet, their utility is directly proportional to how
recently they've been sharpened/honed.
Unlike scissors, the effectiveness of these cutters require a mashing
action between two wedges that are perfectly parallel and precisely
aligned with each other. If there are gaps, nicks, or misalignment
they will not cut cleanly and you might as well throw them away.

I've never known anyone to sharpen them. Removing material will
only make the gaps bigger. I don't think they can be sharpened.

Don
a***@XX.com
2003-12-28 19:10:28 UTC
Permalink
Post by Don K
Post by Alan Horowitz
how to sharpen the mini dike cutters and nipper cutters used in
electrical & electronic work?
They're too small to handle with jigs, and the blades don't even
open very widely. Yet, their utility is directly proportional
to how recently they've been sharpened/honed.
Unlike scissors, the effectiveness of these cutters require a
mashing action between two wedges that are perfectly parallel and
precisely aligned with each other. If there are gaps, nicks, or
misalignment they will not cut cleanly...
Yep! :)
Post by Don K
and you might as well throw them away.
Huh? :/ The handles might get a little closer together but just
about any of them can be fixed up. I use small, thin #4 files
(7/16" wide, 6" long and about 1/16" thick). Nobody I've known
calls them needle files they are wider then needle files. I've
found needle files are too narrow for this job.

My favorite "improvement;)" is to grind the crap out of the "round
face" and make the cutting edges close to the new surface.
Sometimes like for cutting pin material for knife work the round
face and edges are very close, too close for other work. But still
almost all dikes get that treatment at least somewhen they pass
through my hands.

See? I fix up more old junk than just broken pocket knives. :)
Post by Don K
I've never known anyone to sharpen them. Removing material will
only make the gaps bigger. I don't think they can be sharpened.
Don
Don, if you said "I don't think I can sharpen dikes" then I could
agree with you on that one. :) Otherwise, nope. :/

Out of over two dozen sets of dikes I've owned over the years (give
most of them away) only a couple were bought by me brand new. They
can be had (good name brands!) for 50c to a $1 at the swipe and
swap. :) Soak the rusty ones in phosphoric acid first.

When sharpening them you just have to pay attention... Don's -first-
(and excellent) observations above are as good as any.

Just make sure of what effects you are making, in my case...
magnification is the key to success. :)

Alvin in AZ
ps- even an ice pick works better if you sharpen it up sharper
pps- screw drivers too... anything with an edge for that matter
Don K
2003-12-29 02:44:56 UTC
Permalink
Post by a***@XX.com
Don, if you said "I don't think I can sharpen dikes" then I could
agree with you on that one. :) Otherwise, nope. :/
OK, I was wrong to say it can't be done. Obviously, with effort
and a little luck, you might be able to reface the edges to
regain performance over some portion of the cutting edge.

At work, we toss out defective tools so as not to damage
the product.

Don
Carl.
2003-12-28 19:20:20 UTC
Permalink
Post by Don K
Post by Alan Horowitz
how to sharpen the mini dike cutters and nipper cutters used in
electrical & electronic work?
They're too small to handle with jigs, and the blades don't even open
very widely. Yet, their utility is directly proportional to how
recently they've been sharpened/honed.
Unlike scissors, the effectiveness of these cutters require a mashing
action between two wedges that are perfectly parallel and precisely
aligned with each other. If there are gaps, nicks, or misalignment
they will not cut cleanly and you might as well throw them away.
I've never known anyone to sharpen them. Removing material will
only make the gaps bigger. I don't think they can be sharpened.
I suppose it's possible to sharpen the beveled portion, but do it so the tip
gets sharpened more and the very back end not at all, thus making a flush
closure, just with the handles squeezing a little more. That would be a
real PITA though and depending on the tool you might not have much room to
work with. I vote for toss it and get another.


---
Update your PC at http://windowsupdate.microsoft.com
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.556 / Virus Database: 348 - Release Date: 12/26/2003
MaxAluminum
2003-12-28 21:52:07 UTC
Permalink
Post by Carl.
Post by Don K
Post by Alan Horowitz
how to sharpen the mini dike cutters and nipper cutters used in
electrical & electronic work?
They're too small to handle with jigs, and the blades don't even open
very widely. Yet, their utility is directly proportional to how
recently they've been sharpened/honed.
Unlike scissors, the effectiveness of these cutters require a mashing
action between two wedges that are perfectly parallel and precisely
aligned with each other. If there are gaps, nicks, or misalignment
they will not cut cleanly and you might as well throw them away.
I've never known anyone to sharpen them. Removing material will
only make the gaps bigger. I don't think they can be sharpened.
I suppose it's possible to sharpen the beveled portion, but do it so the tip
gets sharpened more and the very back end not at all, thus making a flush
closure, just with the handles squeezing a little more. That would be a
real PITA though and depending on the tool you might not have much room to
work with. I vote for toss it and get another.
---
Update your PC at http://windowsupdate.microsoft.com
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.556 / Virus Database: 348 - Release Date: 12/26/2003
Sharpening them is often an experiment in futility. Give it a try and
then pitch them. Occasionally it works with a Dremel and a small wheel
or carbide tool. And I have a diamond stick that helps a little. In
some you have to remove material in the crotch, for lack of the proper
term, so the tool will close tightly. If you are using the tool for
your livelihood, buy a new quality piece.
a***@XX.com
2003-12-28 22:18:37 UTC
Permalink
Post by MaxAluminum
Sharpening them is often an experiment in futility. Give it a try and
then pitch them. Occasionally it works with a Dremel and a small wheel
or carbide tool.
Oh heck. :/ Using a dremel on the jaws would be a recipe for making
them worse instead of better, in my opinion. I use a small flat #4
file and finish up with a metal finger nail file. (the kind with the
grit soldered to it... either saphire or diamond)
Post by MaxAluminum
And I have a diamond stick that helps a little. In some you have
to remove material in the crotch, for lack of the proper term, so
the tool will close tightly. If you are using the tool for your
livelihood, buy a new quality piece.
I've only ran across one set so far that was so good it couldn't use
touching up, they are little ones for electonic work and they say
"NWS Solingen Germany" on them and the return springs are two little
leaf springs. (instead of those with the crappy little coil spring)

Most of the ones I get and fix up are Kleins but all of them (save
that one set) could use some "hand work" for improvement.

Alvin in AZ
ps- retired/retarded (same thing) railroad signal-ape :)
JC Dill
2003-12-29 05:46:23 UTC
Permalink
Post by a***@XX.com
a metal finger nail file. (the kind with the
grit soldered to it... either saphire or diamond)
Where do you find diamond nail files? I haven't been able to find one
in years. I grew up using diamond nail files (on my nails) and
everything else ("newer" and "improved" not!) feels wrong. I had 3 or
4 of them at one point, and have lost all but 1 over the years. I
would really like to buy at least 2 more, if I could find them!

jc
The Real Bev
2003-12-29 05:51:49 UTC
Permalink
Post by JC Dill
Post by a***@XX.com
a metal finger nail file. (the kind with the
grit soldered to it... either saphire or diamond)
Where do you find diamond nail files? I haven't been able to find one
in years. I grew up using diamond nail files (on my nails) and
everything else ("newer" and "improved" not!) feels wrong. I had 3 or
4 of them at one point, and have lost all but 1 over the years. I
would really like to buy at least 2 more, if I could find them!
Rite-Aid sells something like the Diamond Deb files, but they wear out
sooner.
--
Cheers,
Bev
---------------------------------
aibohphobia - fear of palindromes
Reyd Dorakeen
2003-12-29 06:01:52 UTC
Permalink
some links for diamond nail files.
http://www.cameobeauty.com/Merchant2/merchant.mv?Screen=PROD&Store_Code=Came
o&Product_Code=2111&Category_Code=newpedi
http://www.skincarecatalog.com/tweezerman-diamond-nail-file--3421-p.html
http://www.tropicalshops.com/vcs/Diamond-Nail-File.htm
http://www.dermadoctor.com/product.asp?productid=623
Post by JC Dill
Where do you find diamond nail files? I haven't been able to find one
in years. I grew up using diamond nail files (on my nails) and
everything else ("newer" and "improved" not!) feels wrong. I had 3 or
4 of them at one point, and have lost all but 1 over the years. I
would really like to buy at least 2 more, if I could find them!
jc
JC Dill
2003-12-29 06:13:05 UTC
Permalink
Post by Reyd Dorakeen
http://www.skincarecatalog.com/tweezerman-diamond-nail-file--3421-p.html
WOW! That's it! The other ones aren't the right kind, but this one
is. I haven't seen one like it in years. The last time I tried to
Google to find one all I found were the other type. I'm ordering
several tomorrow. Thanks for the link!

jc
Richard Edward
2003-12-29 06:58:14 UTC
Permalink
-----BEGIN PGP SIGNED MESSAGE-----
Post by JC Dill
Post by a***@XX.com
a metal finger nail file. (the kind with the
grit soldered to it... either saphire or diamond)
Where do you find diamond nail files? I haven't been able to find one
[...]

A long shot, but check your area for bait and tackle shops or sporting
goods stores that carry fishing tackle. Occasionally you'll run across a
pack of diamond files in varrying grits sold as hook sharpeners. The cheap
ones will probably cost about $3 to $5 US. The real diamond files are more
like $15 to $20.
WayLander
2003-12-29 10:40:29 UTC
Permalink
Post by JC Dill
Post by a***@XX.com
a metal finger nail file. (the kind with the
grit soldered to it... either saphire or diamond)
Where do you find diamond nail files? I haven't been able to find one
in years. I grew up using diamond nail files (on my nails) and
everything else ("newer" and "improved" not!) feels wrong. I had 3 or
4 of them at one point, and have lost all but 1 over the years. I
would really like to buy at least 2 more, if I could find them!
jc
Hehehe. That's funny. My wife gets my Leatherman Wave out more often than
I do. To use the diamond file to do her nails!

WayLander


--
Can you feel, I'm not like you anymore?
I can't see, I can't breathe...
It's a bad religion, From a broken nation...
It's a contradiction,
And I can't take it anymore.
~Godsmack


---
Outgoing mail is certified Virus Free.
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.556 / Virus Database: 348 - Release Date: 12/26/2003
Carl.
2003-12-29 12:57:11 UTC
Permalink
Post by JC Dill
Post by a***@XX.com
a metal finger nail file. (the kind with the
grit soldered to it... either saphire or diamond)
Where do you find diamond nail files? I haven't been able to find one
in years. I grew up using diamond nail files (on my nails) and
everything else ("newer" and "improved" not!) feels wrong. I had 3 or
4 of them at one point, and have lost all but 1 over the years. I
would really like to buy at least 2 more, if I could find them!
http://www.eknifeworks.com

Has an EZE-Lap diamond mini file for $3.


---
Update your PC at http://windowsupdate.microsoft.com
Checked by AVG anti-virus system (http://www.grisoft.com).
Version: 6.0.556 / Virus Database: 348 - Release Date: 12/26/2003
Ken Moon
2004-01-01 01:33:18 UTC
Permalink
Post by JC Dill
Post by a***@XX.com
a metal finger nail file. (the kind with the
grit soldered to it... either saphire or diamond)
Where do you find diamond nail files?
*****************************************************
I've been able to find Revlon brand at most department stores, in the beauty
supply area. Also, the large toenail clippers can be used as nippers for
small copper or aluminum wires. As far as the dyke sharpening is concerned,
I've found that a strip of silicon oxide (wet or dry) sandpaper glued to a
"craft stick" (about the size of a popsicle stick, or the larger ones about
the size of a tongue depressor) seems to work well. I have these in various
grits for different projects, but for the purpose here, the 320 to 500 grits
seem to work well for interior sharpening.

Ken Moon
Webberville, TX

Leif Thorvaldson
2003-12-28 21:16:17 UTC
Permalink
How about using those small, flexible sanding disks that one uses with a
Dremel Mototool. I use them for sharpening bandsaw blades mounted on the
bandsaw. Works great for them. You should be able to work them between the
narrow confines of those nippers and dikes!

Leif
Post by Alan Horowitz
how to sharpen the mini dike cutters and nipper cutters used in
electrical & electronic work?
They're too small to handle with jigs, and the blades don't even open
very widely. Yet, their utility is directly proportional to how
recently they've been sharpened/honed.
Chuck
2003-12-28 21:46:58 UTC
Permalink
Post by Alan Horowitz
how to sharpen the mini dike cutters and nipper cutters used in
electrical & electronic work?
They're too small to handle with jigs, and the blades don't even open
very widely. Yet, their utility is directly proportional to how
recently they've been sharpened/honed.
Buy Craftsman or Klien and you wont have to worry about that...
Barry N. Turner
2003-12-29 01:39:41 UTC
Permalink
Alan,

I once tried to sharpen an old pair of diagonal cutters. (I know, not the
same tool, but perhaps the same principle is involved).

I wasn't successful in my sharpening efforts, but I was able to speed up the
need to purchase a new pair quite a bit. After my misguided sharpening
effort, the old ones wouldn't work at all. Heck, there was close to an
eighth inch gap between the jaws when they were fully closed. by the time I
finished.

Almost anything can be done, given enough time and effort, but some things
just aren't worth it. I suspect this project of yours may well be one of
the latter.

Barry
Post by Alan Horowitz
how to sharpen the mini dike cutters and nipper cutters used in
electrical & electronic work?
They're too small to handle with jigs, and the blades don't even open
very widely. Yet, their utility is directly proportional to how
recently they've been sharpened/honed.
JC Dill
2003-12-29 05:50:34 UTC
Permalink
On Sun, 28 Dec 2003 19:39:41 -0600, "Barry N. Turner"
Post by Barry N. Turner
I wasn't successful in my sharpening efforts, but I was able to speed up the
need to purchase a new pair quite a bit. After my misguided sharpening
effort, the old ones wouldn't work at all. Heck, there was close to an
eighth inch gap between the jaws when they were fully closed. by the time I
finished.
Some tools of this type have a "stop" in the jaw, so that when the
stop is closed the blades are almost, but not quite, touching. If you
sharpen the blades on this type of tool you need to grind back the
stop so that when you are done, the edges again *almost* touch.

Hoof nippers (used by farriers) are this type of tool. The good ones
cost ~$150 to buy, and ~$75 to have them rebuilt because of how tricky
it is to sharpen and realign the cutting edges. See:

<http://www.google.com/search?sourceid=navclient&ie=UTF-8&oe=UTF-8&q=GE+nippers+rebuild>

jc